I just became the owner of a Edgun Long Matador in 25 cal…….single shot. I love the stock finish. Dark brown. Just for the heck of it, I was wanting to rub in a few coats of Royal London Oil. Will this adversely affect the factory finish??? Is the factory finish an oil based type? Or a urethane type?
As a side note, I have owned alot of PCP’s over the past few years and this Edgun (I have a 22 cal too…..medium sized) are amazing. Thanks….kevin

EdGun

All Replies

Viewing 2 replies - 1 through 2 (of 2 total)

Thanks Larry. I just want to add a bit of Royal London Oil to the factory finish. According to Ed’s formula……this should work!!!! Thanks Larry, for this great info. I also have a 22 cal Edgun that I used truckbed liner on. I am going to remove that crap and add a drop of ebony to my Rpyal London Oil and see if I can replicate Ed’s look. I love the Edgun. Just knocked out a starling with my 25 cal moments ago. The trigger on my single shot is stiff. It is the trigger with two screws. I’ll watch Ernest’s vid on how to lighten it up a bit. I truly do not know how I have gotten along without an Edgun. Shotcount is awesome……extreme spread is linear……..and very accurate!!!!!! And light. I love it. kevin

Kevin,

Here is ED’s formula!!

Re: Fao of ed regarding beech stocks on edguns
Postby Ed » Sun Apr 19, 2015 7:56 am

We use only walnut. But I never told that I guarantee that it will be absolutely perfect, with very interesting textures, as it is different in blanks. Thus, yes, I admit that one can get very beutuful stock, the other can get ordinary. I never choose which one to send to some specific customer.

So, that is the technical reglament of precessing the stocks:

Standard processing of EDgun stocks:

1. Tinting 01СLТ03538F diluted 1:3 with solvent №646.
2. Drying 24 hours.
3. Impregnation with 00SO50.
4. Drying 24 hours, and polishing with grain №240,320.
5. One layer of oil 00SO30 (40 gloss or 20 gloss.
6. Drying 24 hours and polishing with grain №180,240.
7. Finishing layer of oil 00SO30.
8. Drying 24 hours.

Tinting, impregnation and oil by MAX COLOR.

We used to take so called “american walnut” I didn’t like it as it was too boring 🙂 Now we use walnut from south of Russia, Dagestan region.

With the best regards

Ed
Last edited by Ed on Sun Apr 19, 2015 8:12 am, edited 1 time in total.
User avatar
Ed

Posts: 883
Joined: Tue Feb 19, 2008 12:13 pm
Location: Russia
Regards LarryW 😎

Viewing 2 replies - 1 through 2 (of 2 total)

  • You must be logged in to reply to this topic.